Atenção: Todas as denúncias são sigilosas e sua identidade será preservada.
Os campos nome e e-mail são de preenchimento opcional
Metadados | Descrição | Idioma |
---|---|---|
Autor(es): dc.contributor | Garcia, Fernanda Cristina Pimentel | - |
Autor(es): dc.contributor | Ribeiro, Ana Paula Dias | - |
Autor(es): dc.creator | Poubel, Déborah Lousan do Nascimento | - |
Data de aceite: dc.date.accessioned | 2024-10-23T15:46:38Z | - |
Data de disponibilização: dc.date.available | 2024-10-23T15:46:38Z | - |
Data de envio: dc.date.issued | 2017-03-14 | - |
Data de envio: dc.date.issued | 2017-03-14 | - |
Data de envio: dc.date.issued | 2017-03-14 | - |
Data de envio: dc.date.issued | 2016-11-24 | - |
Fonte completa do material: dc.identifier | http://repositorio.unb.br/handle/10482/22910 | - |
Fonte completa do material: dc.identifier | http://dx.doi.org/10.26512/2016.11.D.22910 | - |
Fonte: dc.identifier.uri | http://educapes.capes.gov.br/handle/capes/891711 | - |
Descrição: dc.description | Dissertação (mestrado) — Universidade de Brasília, Faculdade de Ciências da Saúde, Programa de Pós-Graduação em Ciências da Saúde, 2016. | - |
Descrição: dc.description | A técnica da colagem de fragmento é frequentemente utilizada em casos de fratura coronária para restaurar dentes traumatizados e pode ser influenciada por diferentes tempos de desidratação/reidratação do fragmento. Objetivo: Avaliar a influência dos tempos de desidratação e reidratação do fragmento na resistência à fratura após a colagem, utilizando um sistema adesivo multimodo. Materiais e métodos: Oitenta e quatro incisivos bovinos foram fraturados e randomizados em grupos (n=12). Após a simulação de fratura, cada espécime foi distribuído nos seguintes grupos: G0: controle (dentes hígidos); GA1 e GA2: 1h de desidratação + 15 minutos ou 24h de reidratação, respectivamente; GB1 e GB2: 24h de desidratação + 15 minutos ou 24h de reidratação, respectivamente; e GC: 1h (GC1) ou 24h (GC2) de desidratação. Os fragmentos dentais foram colados, utilizando um adesivo multimodo na técnica autocondicionante com condicionamento ácido seletivo em esmalte, associado a uma resina composta fluida. A resistência à fratura foi avaliada em uma máquina de teste universal, sob força compressiva (1 mm/min-1). Os dados foram submetidos à análise de variância (ANOVA) a dois critérios, seguido de teste Tukey (5%). Resultados: Nenhuma interação estatisticamente significante foi observada entre os períodos de desidratação e reidratação (p>0,05). Apenas o tempo de reidratação aumentou significativamente a resistência à fratura após colagem, quando comparada com grupos submetidos somente à desidratação, independentemente do tempo (15 minutos ou 24h). Conclusão: A reidratação do fragmento dental antes do procedimento de colagem, utilizando um adesivo multimodo, parece devolver a umidade dental suficiente para aumentar os valores de resistência à fratura. | - |
Descrição: dc.description | The tooth fragment bonding technique, frequently used to restore traumatized teeth, may be affected by dehydration/rehydration periods. Objective: To evaluate the effects of different dry and wet storage intervals on multi-mode adhesive bonding between reattached fragments and teeth. Materials and methods: Eighty-four bovine incisors were fractured and randomized into groups (n=12). After teeth fracturing, each specimen was assigned to one of the following groups: G0: control group (sound tooth); GA1 and GA2: 1-h dehydration and a 15-min or 24-h rewetting period, respectively; GB1 and GB2: 24-h dehydration and a 15-min or 24-h rewetting period, respectively; and GC: 1-h (GC1) or 24-h (GC2) dehydration period only. Tooth fragments were reattached using a multi-mode adhesive in a self-mode technique with a flowable resin composite. The fracture resistance was evaluated in a universal testing machine under a compressive load (1 mm/min-1). Data were submitted to two-way analysis of variance and post-hoc Tukey test (5%). Results: No significant interaction between dehydration and rehydration intervals was observed (p>0,05). Only the step of rehydration affected significantly the reattachment strength when compared to the groups only submitted to dehydration, regardless the interval (15 min or 24 h). Conclusion: Rehydrating a tooth fragment before bonding with a multi-mode adhesive appears to maintain sufficient moisture to increase reattachment strength. | - |
Descrição: dc.description | Faculdade de Ciências da Saúde (FS) | - |
Descrição: dc.description | Programa de Pós-Graduação em Ciências da Saúde | - |
Formato: dc.format | application/pdf | - |
Direitos: dc.rights | Acesso Aberto | - |
Direitos: dc.rights | A concessão da licença deste item refere-se ao termo de autorização impresso assinado pelo autor com as seguintes condições: Na qualidade de titular dos direitos de autor da publicação, autorizo a Universidade de Brasília e o IBICT a disponibilizar por meio dos sites www.bce.unb.br, www.ibict.br, http://hercules.vtls.com/cgi-bin/ndltd/chameleon?lng=pt&skin=ndltd sem ressarcimento dos direitos autorais, de acordo com a Lei nº 9610/98, o texto integral da obra disponibilizada, conforme permissões assinaladas, para fins de leitura, impressão e/ou download, a título de divulgação da produção científica brasileira, a partir desta data. | - |
Palavras-chave: dc.subject | Traumatismos dentários | - |
Palavras-chave: dc.subject | Dentes bovinos | - |
Palavras-chave: dc.subject | Dentes - fraturas | - |
Título: dc.title | Influência do tempo de desidratação e reidratação do fragmento dental na resistência à fratura após colagem utilizando sistema adesivo multimodo | - |
Tipo de arquivo: dc.type | livro digital | - |
Aparece nas coleções: | Repositório Institucional – UNB |
O Portal eduCAPES é oferecido ao usuário, condicionado à aceitação dos termos, condições e avisos contidos aqui e sem modificações. A CAPES poderá modificar o conteúdo ou formato deste site ou acabar com a sua operação ou suas ferramentas a seu critério único e sem aviso prévio. Ao acessar este portal, você, usuário pessoa física ou jurídica, se declara compreender e aceitar as condições aqui estabelecidas, da seguinte forma: