Efeito do pré-aquecimento e da vibração ultrassônica na espessura da película formada por compósitos restauradores convencionais utilizados como agente de cimentação: uma análise in vitro através da microtomografia computadorizada

Registro completo de metadados
MetadadosDescriçãoIdioma
Autor(es): dc.contributorFonseca, Edgard de Mello-
Autor(es): dc.contributorhttp://lattes.cnpq.br/4161140131440509-
Autor(es): dc.contributorhttp://lattes.cnpq.br/5432599481393669-
Autor(es): dc.creatorVasques, Wesley Felisberto-
Data de aceite: dc.date.accessioned2024-07-11T18:09:27Z-
Data de disponibilização: dc.date.available2024-07-11T18:09:27Z-
Data de envio: dc.date.issued2023-05-18-
Data de envio: dc.date.issued2023-05-18-
Fonte completa do material: dc.identifierhttp://app.uff.br/riuff/handle/1/28915-
Fonte: dc.identifier.urihttp://educapes.capes.gov.br/handle/capes/764733-
Descrição: dc.descriptionO objetivo deste estudo in vitro foi mensurar e comparar as espessuras das películas de dois cimentos resinosos e duas resinas compostas pré-aquecidas e o efeito da vibração ultrassônica na película formada pelos compósitos pré-aquecidos utilizados como agente de cimentação através da microtomografia computadorizada. Para obtenção dos espécimes foram cimentadas 36 facetas de PMMA sobre modelos plásticos de incisivos centrais com preparos padronizados. Os corpos de prova foram aleatoriamente separados em seis grupos, de acordo com o agente de cimentação (n=6): Variolink Esthetic (VE); RelyX™Veneer (RV); Filtek™Z100 préaquecida (Z100+PA); Estelite Ômega pré-aquecida (EO+PA); Filtek™Z100 préaquecida associada à vibração ultrassônica (Z100+PA+VU); e Estelite Ômega préaquecida associada à vibração ultrassônica (EO+PA+VU). Após a etapa de cimentação, as tomografias foram obtidas utilizando um sistema μTC Skyscan 1273 (Bruker). Depois da digitalização, as imagens foram reconstruídas usando o Software NRecon 1.7.5. A mensuração das espessuras foi realizada utilizando o Software DataViewer. Os dados coletados foram analisados no Software Jamovi versão 2.3.1.0. A distribuição normal dos dados foi avaliada através do teste Shapiro-Wilk. O nível de significância foi estabelecido em 5% (p>0.05). As medidas das espessuras das películas foram submetidas ao teste ANOVA para uma variável, seguido do teste de Tukey. Os resultados demonstraram que as películas mais finas foram as formadas pelos grupos VE (70.4μm) e Z100+PA+VU (84.8μm). As películas mais espessas foram as formadas pelos grupos Z100+PA (209.6 μm) e EO+PA (278.5 μm). As películas produzidas pelos cimentos resinosos VE e RV demostraram diferença estatisticamente significativa entre si. Este estudo concluiu que a associação do pré-aquecimento dos compósitos testados (Filtek Z100 e Estelite Ômega) associados à energia ultrassônica foi capaz de gerar uma película similar à película formada pelo cimento RelyX Veneer.-
Descrição: dc.descriptionThe purpose of this in vitro study was to evaluate and compare the film thickness of tow resin cements and tow preheated restorative composite and effect by the association with the ultrasound energy on the film thickness of preheated restorative composite used as a luting agent through 3-dimensional (3D) microcomputed tomography (mCT). Thirty six plastic veneers were luted on central incisor models with standardized preps (P-Oclusal). The specimens were randomly divided into 6 groups, following the luting agent (n=6): Variolink Esthetic (VE); RelyX™Veneer (RV); preheated Filtek™Z100 (Z100+PA); preheated Estelite Ômega (EO+PA); preheated Filtek™Z100 associated with ultrasound vibration (Z100+PA+VU); and preheated Estelite Ômega associated with ultrasound vibration (EO+PA+VU). After luting steps, the specimens were scanned using a Skyscan 1273 microCT system (Bruker). Following the scanning, the images were reconstructed using NRecon 1.7.5 (Bruker). The film thickness measurement was made in a Software DataViewer. Data were analyzed in Jamovi 2.3.1.0 version. The normal distribution was evaluated by Shapiro-Wilk test (p>0.05). Film thickness measurements were analyzed using one way ANOVA, followed by the Tukey Test. The results showed the thicker films produced by VE (70.4μm) and Z100+PA+VU (84.8μm) groups. The higher films were found on Z100+PA (209.6 μm) and EO+PA (278.5 μm) groups. Film thickness by resin cements groups VE and RV were significantly different (p>0.05). This study concluded that the combination of the ultrasound vibration with the restorative composite preheated tested (Filtek™Z100 e Estelite Ômega) was able to produce a film thickness like the film thickness by the RelyX™Veneer resin cement.-
Descrição: dc.description39 f.-
Formato: dc.formatapplication/pdf-
Idioma: dc.languagept_BR-
Direitos: dc.rightsOpen Access-
Direitos: dc.rightsCC-BY-SA-
Palavras-chave: dc.subjectcimentação-
Palavras-chave: dc.subjectcimento resinoso-
Palavras-chave: dc.subjectresina pré-aquecida-
Palavras-chave: dc.subjectresina termo-modificada-
Palavras-chave: dc.subjectpelícula de cimento-
Palavras-chave: dc.subjectCimentação (Odontologia)-
Palavras-chave: dc.subjectCimento de resina-
Palavras-chave: dc.subjectResina composta-
Palavras-chave: dc.subjectCompósito-
Palavras-chave: dc.subjectluting-
Palavras-chave: dc.subjectresins cement-
Palavras-chave: dc.subjectpreheated composite-
Palavras-chave: dc.subjectfilm thickness-
Título: dc.titleEfeito do pré-aquecimento e da vibração ultrassônica na espessura da película formada por compósitos restauradores convencionais utilizados como agente de cimentação: uma análise in vitro através da microtomografia computadorizada-
Título: dc.titleThe preheated and the ultrasound vibration effect on the restorative composites film thickness using as luting agent: an in vitro 3-dimensional (3D) microcomputed tomography analysis-
Tipo de arquivo: dc.typeTese-
Aparece nas coleções:Repositório Institucional da Universidade Federal Fluminense - RiUFF