Reciclagem de placas de circuito impresso de computadores sucatados para a recuperação de estanho por eletroeluição de resinas poliméricas de troca iônica.

Registro completo de metadados
MetadadosDescriçãoIdioma
Autor(es): dc.creatorMartins, Afonso Henriques-
Autor(es): dc.creatorSilva, Hugo Walisson-
Autor(es): dc.creatorPeres, Antônio Eduardo Clark-
Autor(es): dc.creatorPereira, Carlos Alberto-
Autor(es): dc.creatorTorem, Maurício Leonardo-
Autor(es): dc.creatorDutra, Achilles Junqueira-
Data de aceite: dc.date.accessioned2019-11-06T13:33:23Z-
Data de disponibilização: dc.date.available2019-11-06T13:33:23Z-
Data de envio: dc.date.issued2015-04-07-
Data de envio: dc.date.issued2015-04-07-
Data de envio: dc.date.issued2014-
Fonte completa do material: dc.identifierhttp://www.repositorio.ufop.br/handle/123456789/4951-
Fonte: dc.identifier.urihttp://educapes.capes.gov.br/handle/capes/557992-
Descrição: dc.descriptionEste trabalho apresenta os resultados experimentais para a recuperação de estanho presente em soluções aquosas a parir da reciclagem de computadores sucatados, através da técnica de eletroeluição de resina polimérica catiônica Amberlite IR-120®(Merck, USA). A resina foi carregada pela passagem de 200ml de solução aquosa 0,2g/l de Sn em 2,18N H2SO4 (concentração do licor de lixiviação de placas de circuito impresso-PCI de microcomputadores sucatados) através do leito de 10g de resina. A realização dos experimentos foi baseada em um planejamento estatístico pelo método fatorial completo replicado de três variáveis a dois níveis. A otimização foi feita pelo método do passo ascendente. As condições consideradas ótimas visando a eletrorrecuperação de estanho foram 150A/m2 de densidade de corrente catódica, tempo de eletroeluição de 45 minutos e intensidade de agitação moderada do eletrólito (100rpm). _______________________________________________________________________________-
Descrição: dc.descriptionABSTRACT: This work presents experimental results for tin recovery from synthetic aqueous solution based on leaching liquors for computers recycling using the electroelution technique of cationic polymeric resin Amberlite IR-120® (Merck, USA). The resin was loaded with 200ml of aqueous solution 0.2g/l Sn in 2.18N H2SO4 (same metal content of a leaching liquor of printed circuit board-PCI from scrapped computers) through 10g of polymeric resin bed. The experiments were statistically planned by a replicated full factorial design method for three variables at two levels. The optimization was performed by the ascending path statistical method. The optimum experimental conditions for maximum tin recovery were 150A/m2 for current density, 45 minutes for electroelution and fair stirring intensity around 100rpm.-
Idioma: dc.languagept_BR-
Direitos: dc.rightsO Periódico Holos permite que o Repositório Institucional da Universidade Federal de Ouro Preto (UFOP) deposite uma cópia eletrônica dos artigos publicados por esse periódico em que ao menos um dos autores faça parte da comunidade cientifica da UFOP. Fonte: Licença concedida mediante preenchimento de formulário no dia de 11 mar. de 2015.-
Palavras-chave: dc.subjectEstanho-
Palavras-chave: dc.subjectRecycling-
Palavras-chave: dc.subjectSucata eletrônica-
Palavras-chave: dc.subjectElectroelution-
Palavras-chave: dc.subjectHidrometalurgia-
Título: dc.titleReciclagem de placas de circuito impresso de computadores sucatados para a recuperação de estanho por eletroeluição de resinas poliméricas de troca iônica.-
Título: dc.titleRecycling of printed circuit boards from scrapped computers for tin recovery by electroelution of ion exchange polymeric.-
Aparece nas coleções:Repositório Institucional - UFOP

Não existem arquivos associados a este item.