Flexural strength of a pressable lithium disilicate ceramic: influence of surface treatments

Registro completo de metadados
MetadadosDescriçãoIdioma
Autor(es): dc.contributorUniversidade Estadual Paulista (UNESP)-
Autor(es): dc.creatorSato, Tabata do Prado-
Autor(es): dc.creatorCotes, Caroline-
Autor(es): dc.creatorYamamoto, Lígia Tiaki-
Autor(es): dc.creatorRossi, Natalia Rivoli-
Autor(es): dc.creatorda Cruz Macedo, Vanessa-
Autor(es): dc.creatorKimpara, Estevão Tomomitsu-
Data de aceite: dc.date.accessioned2025-08-21T22:53:03Z-
Data de disponibilização: dc.date.available2025-08-21T22:53:03Z-
Data de envio: dc.date.issued2022-05-02-
Data de envio: dc.date.issued2022-05-02-
Data de envio: dc.date.issued2013-01-01-
Fonte completa do material: dc.identifierhttp://dx.doi.org/10.1186/2196-4351-1-7-
Fonte completa do material: dc.identifierhttp://hdl.handle.net/11449/234407-
Fonte: dc.identifier.urihttp://educapes.capes.gov.br/handle/11449/234407-
Descrição: dc.descriptionThe aim of this paper was to evaluate the influence of different surface treatments on the flexural strength of a pressable lithium disilicate ceramic. Sixteen bars (16x2x4 mm) were made, divided into subgroups (n = 10), and the following surface treatments were done: C - no treatment; H - etching with 5% hydrofluoric acid; HC - etching with 5% hydrofluoric acid, silanization, and cementation; N – etching with 5% hydrofluoric acid, neutralization with supersaturated solution of sodium bicarbonate, silanization, and cementation; U – etching with 5% hydrofluoric acid, ultrasonic cleaning in distillated water, silanization, and cementation; NU - etching with 5% hydrofluoric acid, neutralization with supersaturated solution of sodium bicarbonate, ultrasonic cleaning in distillated water, silanization and cementation. The three points flexural strength was performed 24 h after cementation and the data were analyzed using one-way ANOVA and Tukey’s tests (p-value = 0.05). The results showed that the surface treatment had a significant effect (p-value < 0,05) on the flexural strength of the studied ceramic. The N and NU groups showed lower flexural strength than other groups. Thus, it was concluded that neutralization with supersaturated solution of sodium bicarbonate, followed or not by ultrasonic cleaning results in lower mechanical strength of a pressable lithium disilicate ceramic. The etching with 5% hydrofluoric acid did not reduce the flexural strength of this ceramic type.-
Descrição: dc.descriptionInstitute of Science and Technology UNESP – Univ Estadual Paulista, José Longo, 777, São Dimas-
Descrição: dc.descriptionInstitute of Science and Technology UNESP – Univ Estadual Paulista, José Longo, 777, São Dimas-
Idioma: dc.languageen-
Relação: dc.relationApplied Adhesion Science-
???dc.source???: dc.sourceScopus-
Palavras-chave: dc.subjectDental ceramic-
Palavras-chave: dc.subjectFlexural strength-
Palavras-chave: dc.subjectHydrofluoric acid-
Palavras-chave: dc.subjectSurface treatment-
Título: dc.titleFlexural strength of a pressable lithium disilicate ceramic: influence of surface treatments-