Atenção: Todas as denúncias são sigilosas e sua identidade será preservada.
Os campos nome e e-mail são de preenchimento opcional
Metadados | Descrição | Idioma |
---|---|---|
Autor(es): dc.contributor | Universidade Estadual Paulista (Unesp) | - |
Autor(es): dc.contributor | Universiteit van Amsterdam and Vrije Universiteit. | - |
Autor(es): dc.creator | de Carvalho, Ana Beatriz Gomes [UNESP] | - |
Autor(es): dc.creator | Dal Piva, Amanda Maria de Oliveira [UNESP] | - |
Autor(es): dc.creator | Tribst, João Paulo Mendes [UNESP] | - |
Autor(es): dc.creator | Werner, Arie | - |
Autor(es): dc.creator | Saavedra, Guilherme de Siqueira Ferreira Anzaloni [UNESP] | - |
Autor(es): dc.creator | Kleverlaan, Cornelis Johannes | - |
Data de aceite: dc.date.accessioned | 2022-02-22T00:31:52Z | - |
Data de disponibilização: dc.date.available | 2022-02-22T00:31:52Z | - |
Data de envio: dc.date.issued | 2020-12-11 | - |
Data de envio: dc.date.issued | 2020-12-11 | - |
Data de envio: dc.date.issued | 2020-10-31 | - |
Fonte completa do material: dc.identifier | http://dx.doi.org/10.1016/j.jmbbm.2020.104009 | - |
Fonte completa do material: dc.identifier | http://hdl.handle.net/11449/200838 | - |
Fonte: dc.identifier.uri | http://educapes.capes.gov.br/handle/11449/200838 | - |
Descrição: dc.description | This study compared the wear resistance of different reinforced glass-ceramics crystalized by conventional or microwave firing. The wear rate of three ceramics [one lithium disilicate ceramic (LD): IPS e.max CAD – Ivoclar Vivadent; and two zirconia reinforced lithium silicates: Suprinity – VITA Zahnfabrik (ZLS1) and Celtra Duo – Dentsply (ZLS2)] crystallized by conventional (c) or microwave (mw) firing protocols were collected according to the contact- [two-body (n = 20/gr)] and contact-free wear tests [three-body (n = 20/gr)]. After wear tests performed on ACTA wear machine, mean surface roughness (Ra) and Scanning Electron Microscopy (SEM) analyzes were performed to evaluate the surface alterations. The wear and roughness data (in μm) were evaluated using two-way ANOVA and Tukey post-hoc test (α = 0.05). Two-body wear test revealed that ZLS1 (1.30 ± 1.79)A showed higher wear rate than LD (0.79 ± 2.15)B and ZLS2 (0.85 ± 0.94)B, regardless the crystallization approach. For three-body test, conventional crystallization (0.62 ± 0.4)A showed higher wear rates than microwave (0.22 ± 0.71)B; while the type of ceramic was not significant. The crystallization protocol (p < 0.001) and ceramic material (p = 0.001) affected the surface roughness in the three-body; whereas the two-body test, only the crystallization protocol (p = 0.046). SEM analysis showed a similar and smother surface morphology for LD and ZLS2 compared to ZLS1. Conventional crystallization showed materials more prone to wear than the microwave, in the presence of food bolus. Therefore, the microwave crystallization can be suggested as an alternative to improve the evaluated glass-ceramics wear resistance. | - |
Descrição: dc.description | Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP) | - |
Descrição: dc.description | Post-Graduate Program in Restorative Dentistry (Prosthodontic) Department of Dental Materials and Prosthodontics São Paulo State University (Unesp/SJC) Institute of Science and Technology, Engenheiro Francisco José Longo Avenue, 777 | - |
Descrição: dc.description | Department of Dental Materials Science Academic Centre for Dentistry Amsterdam (ACTA) Universiteit van Amsterdam and Vrije Universiteit., Gustav Mahlerlaan #3004 | - |
Descrição: dc.description | Post-Graduate Program in Restorative Dentistry (Prosthodontic) Department of Dental Materials and Prosthodontics São Paulo State University (Unesp/SJC) Institute of Science and Technology, Engenheiro Francisco José Longo Avenue, 777 | - |
Descrição: dc.description | FAPESP: 2019/06458-5 | - |
Idioma: dc.language | en | - |
Relação: dc.relation | Journal of the Mechanical Behavior of Biomedical Materials | - |
???dc.source???: dc.source | Scopus | - |
Palavras-chave: dc.subject | ACTA wear machine | - |
Palavras-chave: dc.subject | Dental ceramics | - |
Palavras-chave: dc.subject | microwave processing | - |
Título: dc.title | Effect of microwave crystallization on the wear resistance of reinforced glass-ceramics | - |
Tipo de arquivo: dc.type | livro digital | - |
Aparece nas coleções: | Repositório Institucional - Unesp |
O Portal eduCAPES é oferecido ao usuário, condicionado à aceitação dos termos, condições e avisos contidos aqui e sem modificações. A CAPES poderá modificar o conteúdo ou formato deste site ou acabar com a sua operação ou suas ferramentas a seu critério único e sem aviso prévio. Ao acessar este portal, você, usuário pessoa física ou jurídica, se declara compreender e aceitar as condições aqui estabelecidas, da seguinte forma: