Alternating current oxidation of Ti-6Al-4V alloy in oxalic acid for corrosion resistant surface finishing

Registro completo de metadados
MetadadosDescriçãoIdioma
Autor(es): dc.contributorUniversidade de São Paulo (USP)-
Autor(es): dc.contributorUniversidade Estadual Paulista (Unesp)-
Autor(es): dc.contributorMetrohm Autolab BV-
Autor(es): dc.creatorBandeira, Rafael Marinho-
Autor(es): dc.creatorRego, Galtiere Correa-
Autor(es): dc.creatorPicone, Carlos Alberto [UNESP]-
Autor(es): dc.creatorvan Drunen, Julia-
Autor(es): dc.creatorCorrer, Wagner Rafael-
Autor(es): dc.creatorCasteletti, Luiz Carlos-
Autor(es): dc.creatorSpinola Machado, Sergio A.-
Autor(es): dc.creatorTremiliosi-Filho, Germano-
Data de aceite: dc.date.accessioned2022-02-22T00:20:53Z-
Data de disponibilização: dc.date.available2022-02-22T00:20:53Z-
Data de envio: dc.date.issued2020-12-10-
Data de envio: dc.date.issued2020-12-10-
Data de envio: dc.date.issued2020-06-01-
Fonte completa do material: dc.identifierhttp://dx.doi.org/10.1007/s42452-020-2905-y-
Fonte completa do material: dc.identifierhttp://hdl.handle.net/11449/197802-
Fonte: dc.identifier.urihttp://educapes.capes.gov.br/handle/11449/197802-
Descrição: dc.descriptionIn this work, alternating current (AC) voltage (V-AC) is applied to Ti-6Al-4V alloy in aqueous oxalic acid dihydrate solution to grow passive oxide films. The oxide layers are formed with V-AC values in the range of 10-80 V. The resulting surface oxide layers have estimated thicknesses in the 100-500 nm range and are expected to have a two-layer structure consisting of a porous outer layer and a compact inner layer. The AC anodization process is demonstrated to have a slight effect on the surface roughness. Porous regions are observed on the films formed at lower and high AC voltages (i.e., V-AC 10-30 and 80 V). The corrosion behavior in Ringer's solution over 48 h of exposure is studied with electrochemical impedance spectroscopy. The AC anodized samples have higher impedance values than the untreated alloy by more than an order of magnitude. The oxides formed at V-AC = 40 - 70 V exhibit optimal resistance to corrosion as demonstrated by the overall impedance values, the polarization resistance values, and the capacitive behavior.-
Descrição: dc.descriptionCoordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)-
Descrição: dc.descriptionUniv Sao Paulo, Inst Quim Sao Carlos, BR-13566590 Sao Carlos, SP, Brazil-
Descrição: dc.descriptionUniv Sao Paulo, Escola Engn Sao Carlos, BR-13566590 Sao Carlos, SP, Brazil-
Descrição: dc.descriptionUniv Estadual Paulista Julio Mesquita, Fac Engn Ilha Solteira, BR-15385000 Ilha Solteira, SP, Brazil-
Descrição: dc.descriptionMetrohm Autolab BV, Kanaalweg 29-G, NL-3526 KM Utrecht, Netherlands-
Descrição: dc.descriptionUniv Estadual Paulista Julio Mesquita, Fac Engn Ilha Solteira, BR-15385000 Ilha Solteira, SP, Brazil-
Descrição: dc.descriptionCAPES: 001-
Formato: dc.format14-
Idioma: dc.languageen-
Publicador: dc.publisherSpringer-
Relação: dc.relationSn Applied Sciences-
???dc.source???: dc.sourceWeb of Science-
Palavras-chave: dc.subjectAC anodization-
Palavras-chave: dc.subjectTi-6Al-4V alloy-
Palavras-chave: dc.subjectOxide film-
Palavras-chave: dc.subjectCorrosion-
Título: dc.titleAlternating current oxidation of Ti-6Al-4V alloy in oxalic acid for corrosion resistant surface finishing-
Tipo de arquivo: dc.typelivro digital-
Aparece nas coleções:Repositório Institucional - Unesp

Não existem arquivos associados a este item.